Skip to product information
  • Sku: HTLF04

4 in 1 Headlight Film Kit with Air Channel Paper Liner

$229.00 USD
 per 
In stock!
Size

View full details

4 in 1 Headlight Film Kit with Air Channel Paper Liner

Description

Key Features

  • Air Channel for Easy Installation: Integrated air channels allow for bubble-free installation.
  • Anti-Scratch Top Protected Film: Top film layer protects against scratches and keeps the surface smooth.
  • Dry Application: No water needed; easily applied with a dry method.
  • Repositionable: Allows for multiple adjustments during installation.
  • High Clarity: Ensures high transparency for clear visibility.

Structure

  1. Gloss Finish (4 layers): Top Protected Film, Polymeric Face Film, Acrylic Adhesive, Release Liner.
  2. Satin Finish (3 layers): Polymeric Face Film, Acrylic Adhesive, Release Liner.

Specifications

Set of 4 Colors: Golden Yellow, Light Black, Deep Black, Satin Black

Size: 32ft(L) x 1.31ft(W)

Durability: 1 year

Recommendations

  • Recommended Application Tools: Squeegee, buffer, knife, masking tape, heat gun, magnets, gloves, IRR thermometer, sprayer, towel, and installation liquid
  • Application Method: Standard methods for Car Light Protection Film. Do not overstretch and overheat. Post heating is necessary.
  • Post-heating Temperature: 110°C flat surfaces, 130°C curves and overlaps.
  • Aftercare: PH neutral. Avoid wax or solvents.

Physical Properties 

Classification Unit Spec Remark

Thickness

Top protected film um 25±5

PE

Face Film um 100±5

/

Acrylic Adhesive um 20±2 Solvent-based

Release liner

um 180±2 Paper Liner
Surface / / Glossy & Matte /
Width / cm 30/40±0.01% 1ft/1.3ft
Length / m 10±1% 32ft


Physical Performance

Features Test Method/Conditions Results
Gloss (60°) GB 8807 92.3
VLT / 87%
Peel Strength
N/25mm
180° 15
Self-healing Layer Elongation at Break GB/T 1040.1 112
Face Film Elongation at Break GB/T 1040.1 309.5
Tear Strength GB/T529 92.7 KN/m
Tensile Strength GB/T 1040.1 21.6 Mpa
Holding power(h) paste on steel board, hang on by 25mm*25mm*1kg weight under 29℃ and 55%, GB/T4851-1998 48H No Peeling
Aging Test  65℃ and 7 days No adhesive residue under 20 times wrapping
100% Modulus GB/T 1040.1 9.1 Mpa
Initial Tack(g /25mm) under 24℃ and 26%, GB31125-2014 860
Release Force (N/25mm) paste on steel board, 90° 26℃ and 60%, GB2792 0.16
Application Temperature / +20℃ to +30℃
Service Temperature / -50℃ to +110℃
Recommended Shelf Life 72°F (22°C) and 50% RH 1 year
Durability / 1 year

Important Notice

The physical properties of the product detailed in this document are based on tests that we believe to be reliable. They are intended only as a source of information and are given without guarantee. They do not constitute a warranty. Purchasers should independently assess the suitability of this material for their specific use prior to application.

Warranty, Limited Remedy, and Disclaimer

Unless an additional warranty is specifically stated on the applicable product packaging or literature, VinylFrog warrants that each product meets the applicable specifications at the time of shipment. We make no other warranties or conditions, express or implied, including but not limited to any implied warranty or condition of merchantability or fitness for a particular purpose, or any implied warranty or condition arising out of a course of dealing, custom, or usage of trade. If the VinylFrog product does not conform to this warranty, then based on our discretion, the sole and exclusive remedy is either the replacement of the product or a refund of the purchase price.

Limitation of Liability

Except where prohibited by law, VinylFrog will not be liable for any loss or damage arising from its product, whether direct, indirect, special, incidental or consequential, regardless of the legal theory asserted, including warranty, contract, negligence or strict liability.

Durability

The durability of the product is based on exposure conditions in South China. Actual performance life will depend on substrate preparation, exposure conditions, and maintenance of the product. For instance, in areas with excessively high temperature, industrial pollution, or high altitude, exterior performance will decrease.